Microstructure Evaluation and Low Cycle Fatigue Damage due to Degradation of Ni-based Superalloy
니켈기 초내열합금의 열화에 따른 미세구조 및 저주기 피로손상도 평가
Inkang Heo, Donghyun Yoon, Sanghyun Hong, Jinyeol Kim, Jaehoon Kim, Sungho Chang, Siyeon Bae
허인강, 윤동현, 홍상현, 김진열, 김재훈, 장성호, 배시연
Korean J. Met. Mater. 2018;56(8):561-569.   Published online 2018 Aug 5
DOI: https://doi.org/10.3365/KJMM.2018.56.8.561

Abstract
Nickel-based superalloys have excellent resistance to extreme environments such as high temperature and high stress and are used as materials for large gas turbines. In this paper, specimens were taken from a blade that had been used for a long time, and their life span was studied by analysis of microstructure...... More

                           Cited By 2
Characterization of Microstructures and Creep Fracture Characteristics of Dissimilar Metal Welds between Inconel 740H Ni-Based Superalloy and Gr.92 Ferritic Steel
니켈기 Inconel 740H 초내열합금과 고Cr계 Gr.92 내열강의 이종금속 용접부의 미세조직 및 크리프 파단 특성
Kyeong-Yong Shin, Ji-Won Lee, Jung-Min Han, Kyong-Woon Lee, Byeong-Ook Kong, Hyun-Uk Hong
신경용, 이지원, 한정민, 이경운, 공병욱, 홍현욱
Korean J. Met. Mater. 2018;56(5):375-383.   Published online 2018 May 8
DOI: https://doi.org/10.3365/KJMM.2018.56.5.375

Abstract
Microstructure evolution and the creep fracture characteristics of dissimilar welds between Ni-based superalloy Inconel 740H and High Cr ferritic steel Gr.92 were investigated. The dissimilar welds were fabricated by shielded metal arc (SMA) welding process with Ni-based austenitic Inconel 182 superalloy. Postweld heat treatment at 760 oC for 4 hours..... More

         Cited By 5
1 |
E-Submission
Email Alert
Author's Index
Specialties
Impact factor
The Korean Institute of Metals and Materials
SCImago Journal & Country Rank
Scopus
GoogleScholar
Similarity Check
Crossref Cited-by Linking
KOFST
COPE
Editorial Office
The Korean Institute of Metals and Materials
6th Fl., Seocho-daero 56-gil 38, Seocho-gu, Seoul 06633, Korea
TEL: +82-2-557-1071   FAX: +82-2-557-1080   E-mail: metal@kim.or.kr
About |  Browse Articles |  Current Issue |  For Authors and Reviewers
Copyright © The Korean Institute of Metals and Materials.                 Developed in M2PI