Korean J. Met. Mater. 2020;58(7):488-494. Published online 2020 Jul 5
DOI:
https://doi.org/10.3365/KJMM.2020.58.7.488
Abstract
Cu-Ni-Si alloys were strengthened by Ni
2Si intermetallic compound precipitation in a Cu matrix during aging. The Cu-6 wt% Ni-1.4wt%Si alloy was prepared by water quenching (solution treatment) or air cooling (homogenization treatment) after heating 980
oC for 2 hours and aging at 500
oC for 6 hours. After maintaining a.....
More